Physical Properties |
Typical Value |
SI . Unit |
Test Condition |
Test Standard |
| Density | 1.2 | g/cm³ | 23°C | ISO 1183 |
| Melt Flow Rate | 10 | g/10 min | 300°C/1.2 kg | ISO 1133 |
| Molding shrinkage | 0.2~0.7 | % | Parallel | Internal methods |
| Molding shrinkage | 0.2~0.6 | % | Normal | Internal methods |
| Weather resistance | F1 | - | UV, Water Exposure / Immersion | UL 746C. |
Mechanical Properties |
Typical Value |
SI . Unit |
Test Condition |
Test Standard |
| Tensile stress | 60 | MPa | 23°C,50mm/min,yield | ISO 527-2 |
| Tensile modulus | 2300 | MPa | 23°C | ISO 527-2 |
| Strain at break | >50% | % | 5mm/min brk | ISO 527-2 |
| Flexural stress | 86 | MPa | 2mm/min | ISO 178 |
| Flexural modulusress | 2300 | MPa | 2mm/min | ISO 178 |
| Charpy notched impact strength | 58 | KJ/M² | 23°C | ISO 179-1 |
| Charpy notched impact strength | 10 | KJ/M² | -30°C, in 10s | ISO 179-1 |
| Izod notched impact strength | 58 | KJ/M² | 23°C | ISO 180 |
Thermal Properties |
Typical Value |
SI . Unit |
Test Condition |
Test Standard |
| Temperature of deflection under load | 133 | °C | 0.45 MPa, 4 mm | ISO 75-2 |
| Temperature of deflection under load | 120 | °C | 1.8 MPa, 4 mm | ISO 75-2 |
| Vicat softening temperature | 140 | °C | B 50N | ISO 306 |
Electrical Properties |
Typical Value |
SI . Unit |
Test Condition |
Test Standard |
| Insulation resistance | ≥10E6 | MΩ | 23°C 50%RH ;DC 1KV,60S | IEC 62631-3-3:2015 |
| Withstand voltage leakage current | <0.5 | mA | 23°C 50%RH ;AC 3KV,60S | IEC 60243-1:2013 |
| Surface resistivity | 1E+16 | ohms | 23°C | IEC 60093 |
| Volume resistivity | 1E+16 | ohms*cm | 23°C | IEC 60093 |
| Inclined-Plane Tracking | 1500 | V | 3mm | GB/T 6553-2014 |
| Comparative Tracking Index | 600 | V | 23°C | UL 746A |
Flammability Properties |
Typical Value |
SI . Unit |
Test Condition |
Test Standard |
| Flame class | V-0 | - | 1.5mm | UL94 |
| Flame class | HB | - | 0.75mm | UL94 |
Processing Conditions |
Typical Value |
SI . Unit |
||
| Drying temperature | 120 | °C | ||
| Drying time | 4 | hr | ||
| Rear zone temp. | 245~260 | °C | ||
| Middle zone temp. | 255~270 | °C | ||
| Front zone temp. | 260~280 | °C | ||
| Nozzel temp. | 260~295 | °C | ||
| Special instructions [1] ,..The TDS provided here is based on our existing knowledge and experience which has been tested in our materials laboratory. We can guarantee the authenticity of the test result. [2] ,.,,,,,,,.The data provided in TDS only represents the typical value of the product and should not be used as the technical certificate of the material. Since human, machine, material, method, environment and other factors during material processing and testing will affect the judgment and application of materials, this TDS only provides technical reference for engineers in selection or processing. In order to achieve the expected effect of your company, it is necessary to conduct experiments. [3] ,,.,.The shrinkage value provided in TDS is measured according to the international standard shrinkage film, which will be different from the tooling shrinkage of the actual product. So that the shrinkage value is only used for reference. If you need sample resines, please contact the relevant personnel of our company. [4] ,,,/.Pigments may affect the properties , unless otherwise specified, the data in TDS represent the properties of the naturel /black color material. [5] ,,,.With the accumulation of our knowledge and experience, the TDS will be updated constantly. In order to obtain the latest version please contact our sales and service personnel directly. |
||||